Possible causes |
Ways of avoiding it |
---|---|
A paint run is the result of an excess of dilution or the employment of an excessively slow solvent |
Use the suitable paint thinner, in accordance with the type and temperature of the painting surface (according to technical datasheet) |
Application of an excessively thick layer |
The surface should not be applied so much paint |
The paint is too thick |
Increase the brushability with solvent and by shaking |
Intense direct sunlight causes a superficial drying of the paint and subsequent slippage in vertical surfaces |
Avoid direct sunlight or apply thinner layers |
Unequal distribution of finish using a gun |
Apply the paint with the gun using regular and parallel movements |
The use of an unsuitable air cap, projecting an excessive film |
Use the air cap recommended in the technical datasheet |
MAIN OFFICES
C/ San Fernando, 116
26300 Nájera, La Rioja (Spain)
T.: (+34) 941 410 000
F.: (+34) 941 410 111
SOCIAL NETWORKS
CONTACT YOUR NEAREST LOCAL OFFICE
T.: (+34) 941 410 000
delegations-barpimo-spainDelegations Barpimo Spain
LOCATE OUR DISTRIBUTORS
BARPIMO S.A.
C/ SAN FERNANDO, 116
CP: 26300 NÁJERA (LA RIOJA)
T.: (+34) 941 410 000
CONTACT SAC (Customer Service Department)
Barpimo S.A. has always focused its efforts on total quality, thus complying with the obligation of a leader in terms of products and services for the customer.
MAIN SAC DEPARTMENT:
T.: (+34) 941 410 000
sac@barpimo.com